ASSAB XW-42

KETAHANAN AUS TINGGI SEHINGGA MENGHASILKAN MASA PAKAI PANJANG PERKAKAS UNTUK DITERAPKAN DI TEMPAT PENGAUSAN MENJADI MASALAH UTAMA

ASSAB XW-42

  • Abrasive wear resistance 55%
  • Adhesive wear resistance 25%
  • Ductility/edge chipping resistance 20%
  • Toughness/gross cracking resistance 10%

W.nr 1.2379, AISI D2

  • Ketahanan aus abrasi 55%
  • Ketahanan aus adhesif 25%
  • Elastisitas/ketahanan penyerpihan sisi 20%
  • Kekukuhan/ketahanan retakan kasar 10%

Designations

Chemical composition

C 1,55 Si 0,30 Mn 0,40
Cr 11,30 Mo 0,80 V 0,80