VIDAR SUPERIOR
ĐƯỢC PHÁT TRIỂN VỚI ĐỘ DAI VƯỢT TRỘI
VIDAR SUPERIOR
- Hot wear resistance 40%
- Plastic deformation resistance 50%
- Heat checking resistance 60%
- Premature cracking resistance 85%
Reference steel AISI H13
- Hot wear resistance 40%
- Plastic deformation resistance 40%
- Heat checking resistance 40%
- Premature cracking resistance 35%
Designations
Thành phần hóa học
| C | Si | Mn | Cr | Mo | V |
|---|---|---|---|---|---|
| 0,36 | 0,30 | 0,30 | 5,00 | 1,30 | 0,50 |