VIDAR SUPERIOR
DEVELOPED TO BE TOUGH
VIDAR SUPERIOR
- Hot wear resistance 40%
- Plastic deformation resistance 50%
- Heat checking resistance 60%
- Premature cracking resistance 85%
Reference Grade
- Hot wear resistance 40%
- Plastic deformation resistance 40%
- Heat checking resistance 40%
- Premature cracking resistance 35%
Designations
Chemical composition
C | 0.36 | Si | 0.30 | Mn | 0.30 |
Cr | 5.00 | Mo | 1.30 | V | 0.50 |