SKOLVAR
FOR SUPERIOR HOT FORMING TOOLS
SKOLVAR
- Hot wear resistance 90%
- Plastic deformation resistance 80%
- Heat checking resistance 30%
- Premature cracking resistance 15%
Reference Grade
- Hot wear resistance 40%
- Plastic deformation resistance 40%
- Heat checking resistance 40%
- Premature cracking resistance 35%
Designations
Chemical composition
C | 0.70 | Si | 0.20 | Mn | 0.45 |
Cr | 5.00 | Mo | 2.25 | V | 1.60 |